MEMSnet Home: MEMS-Talk: SU-8 Developing Issue, advice required
SU-8 Developing Issue, advice required
2005-04-20
Nan Xie
2005-04-20
Hongjun-ECE
2005-04-20
Brubaker Chad
2005-04-20
chong hanwoo
2005-04-21
Dwayne Dunaway
SU-8 Developing Issue, advice required
Nan Xie
2005-04-20
Hi,

I am developing SU-8 2050 after spun around 50um.
My procedures for soft baking, exposure, and PEB are correct.
I am having trouble getting clean develops after about 6min and 2-3s acetone
spray.
What I am getting are some milky residue around my features. I understand I need
to develop it more when this occurs, but this milky residue still remains or the
SU-8 would come off.

Anyone have any suggestions? Maybe I need to expose more?

Thank you very much,

Nan Xie

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Addison Engineering