AW: Anodic bonding oxidized Silicon wafers to Glass
2005-04-21
Cetin, Volkan
AW: Anodic bonding oxidized Silicon wafers to Glass
Cetin, Volkan
2005-04-21
Hello Charles,

It should be possible to bond a oxidized silicon wafer with glass. But keep
in mind that oxide is an insulating layer, hence it will lower your electric
field at interface. This means for you that a higher voltage and temperature
is necessary in comparison to standard anodic bonding (Si-Glass). Of course
the optimum voltage and temperature is depending on the thickness of your
oxide layer and kind of oxide (PECVD- or thermal oxide?). For 200nm I would
apply -1000V at 400C, if it does not work then increase the voltage. Another
drawback will be the bonding time, it will take longer to bond.


Best Regards,
Volkan Cetin

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing