A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SiO2 As a Mask
SiO2 As a Mask
2005-04-17
guda reddy
2005-04-18
David Nemeth
2005-04-18
[email protected]
2005-04-18
Shile
2005-04-18
Kenneth Smith
2005-04-21
guda reddy
2005-04-21
David Nemeth
2005-04-21
Joe Lonjin
SiO2 As a Mask
Joe Lonjin
2005-04-21
I would support the others comments, all of our v-groove etching and
through wafer etching were with Nitride, simply because it is the better
mask. Thicker oxide begins to develop problems, and for us there is no
downside to Nitride, we simply deposit nitride instead of oxide.

Regards,

Joe Lonjin
Penn State Nanofabrication Facility

-----Original Message-----
From: guda reddy [mailto:[email protected]]
Subject: [mems-talk] SiO2 As a Mask

Hi,
      Thank you guys for replying to my previous mail. What iam trying
to do was to make use of the silicon wafers with the grown oxide layer
to fabricate deep v-grooves using KOH. As you all know that one micro
thick is not sufficent enough to make deep grooves. I can go a head and
change the mask to silicon nitride, but before doing that i wanted to
know why can't we grow thicker oxide layers and use it for deeper
grooves. I am trying to look for some books or papers that gives me some
solid proof that i have change the my mask. If any of you guys can
mention the books or papers that i am looking for would be really
helpful and i would really appriciate for your help.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics