MEMSnet Home: MEMS-Talk: Questions about DC-bias in dry etching
Questions about DC-bias in dry etching
2005-04-21
xiaodong wang
2005-04-22
William Lanford-Crick
2005-04-21
xiaodong wang
2005-04-22
Paolo Tassini
2005-04-21
[email protected]
2005-04-22
xiaodong wang
2005-04-22
xiaodong wang
Questions about DC-bias in dry etching
William Lanford-Crick
2005-04-22
Some ideas RE DC-bias from our experience:
Chamber cleanliness:  Deposition onto top electrode sidewalls of chamber
can lower the DC bias.
Carrier wafer: You mention size of carrier wafer, but material *type* of
carrier wafer should be consistent--it effects the bias.
Do you have cooling water in the lower electrode?  If so, check the
resistivity of the water, if possible.  It should be de-ionized.  We
once put city water in as cooling water, and found that the DC bias
dropped significantly.  We currently use a recirculating chiller with
filters.

Hope this helps,
Bill

-----Original Message-----
From: xiaodong wang
Subject: [mems-talk] Questions about DC-bias in dry etching

Dear all,

I have questions about DC-bias in dry etching.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Nano-Master, Inc.
Tanner EDA by Mentor Graphics