MEMSnet Home: MEMS-Talk: The most minimum thickness of SU8 spin coating?
The most minimum thickness of SU8 spin coating?
2005-04-23
Siripon Sukuabol
2005-04-24
[email protected]
2005-04-25
Jiang Ziling
The most minimum thickness of SU8 spin coating?
Jiang Ziling
2005-04-25
hi siripon,

  There is a su-8 thinner that can thin su-8 down to any thickness you
want. you buy it from microchem and mix it with your su-8 by a certain
ratio, then it can be used.

 cheers

 Jiang Ziling

On 4/23/05, Siripon Sukuabol  wrote:
> Dear All,
> Please give me your advise and lab. experiment.
> What is the most minimum thickness that can get from SU-8 spin coating?
> Is it possible for SU-8 thickness of 0.3um?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.