MEMSnet Home: MEMS-Talk: su-8 air bubble problem
su-8 air bubble problem
2005-04-30
Jiang Ziling
2005-04-30
Dominik Weiland
2005-04-30
Jan Oberthür
2005-04-30
Minghai Li
2005-04-30
Joseph Grogan
Young's modulus
2005-04-30
srinivasan
2005-05-03
Brubaker Chad
2005-05-05
[email protected]
su-8 air bubble problem
Dominik Weiland
2005-04-30
Hi,

There is a Swiss company called Gersteltec selling SU-8.
In their datasheet www.gersteltec.ch they propose to use a thin tip to open
the air bubbles and then allow for a long relaxation time up to a day for
the SU-8 to flow into the gaps produced.
I tried it and it worked for me.

Dominik Weiland


-----Original Message-----
From:  Jiang Ziling
Subject: [mems-talk] su-8 air bubble problem

  I am using Su-8 and frequently there are air bubbles left in the film
after spin coating. It is more serious with thicker films. I tried to get
rid of them by putting the pre-spinning resist-coated wafer in vacuum
dessicator, but the bubbles won't go. Anyone have experience in this?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
University Wafer
The Branford Group