Maria Nordstrom
2005-05-03
Dear Zhiyan,

We have done a detailed study of the adhesion between SU-8 and metal and
I send you a copy of the article. Unfortunately, we did not investigate
how to improve the adhesion between SU-8 and Cu, but I can refer you to
work done by J. Ge and J.K. Kivilahti published in Journal of Applied
Physics 92(6) (2002) 3007-3015.

I hope you will find our study useful!

Sincerely,
Maria Nordstr
PhD Student, Bioprobe Group
MIC - Department of Micro and Nanotechnology
Technical University of Denmark
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing