Rihui He
2005-05-04
Isaac Wing Tak Chan
2005-05-05
[email protected]
photoresist or polyimide sacrificial layer
Rihui He
2005-05-03
Dear all,

I am planning to use AZ 4620 or AZ 4330 as sacrificial layer for my metal
device. Are they easy to reflow to form a round edge? Or I may get better result
by using polyimide?

Best regards,

Rihui He