319 developer while protecting Al
[email protected]
2005-05-05
Zhaoyan,

Have you tried using AZ developer? there's also a company called Clariant.
Best Regards

Tony

-----Original Message-----
From: Zhaoyang Fan 
Subject: [mems-talk] 319 developer while protecting Al

Hello,

We use Shipley 319 photoresist developer, while it attack the bottom Al metal
layer. Could you give me some advices how to overcome this problem? Any other
developers?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
MEMStaff Inc.
Addison Engineering