A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: About Negative Photoresist
About Negative Photoresist
2005-05-08
[email protected]
2005-05-09
Kristjan Leosson
2005-05-09
Brubaker Chad
2005-05-09
Brubaker Chad
2005-05-11
[email protected]
About Negative Photoresist
Brubaker Chad
2005-05-09
Kristjan,

I'm not sure if that is correct.  Negative tone resists work by becoming
cross-linked (i.e., less soluble) when exposed to UV.  So, the flood
exposure process you described would just be re-exposing the regions
that were already exposed the first time around (since the pattern is
there due to the fact that it was exposed in the first round).

Best Regards,
Chad Brubaker

 -----Original Message-----
From: Kristjan Leosson
Subject: RE: [mems-talk] About Negative Photoresist

You can use maN-490 from www.microresist.de for film thickness in the
range 5-16um. Since it is a negative resist, you can use flood exposure on
the final pattern and remove it with your standard developer.  You can
also use organic solvents.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.