MEMSnet Home: MEMS-Talk: Wet-Etch SiO2/Si3N4
Wet-Etch SiO2/Si3N4
2005-05-12
Josef Kouba
2005-05-12
[email protected]
2005-05-12
Brent Garber
2005-05-12
[email protected]
Wet-Etch SiO2/Si3N4
Brent Garber
2005-05-12
J,

Buffered HF

B

Josef Kouba wrote:

> what is a good wet etchant for SiO2 which leaves Si3N4 intact?
reply