You could purchase from SouthBay Technology, a Model 150 lapping and
polishing fixture, a glass plate and appropriate consumables and do it
yourself. Do say 9 micron aluminum oxide abrasive first and then clean
and remount for 3, 1, and 0.3 progressively. You should be able to get a
specular surface.

Thomas Wilson
Marshall Physics

-----Original Message-----
From:  Ho Yin Chan
Subject: [mems-talk] Quartz wafer polishing surface

I have a package of quartz wafers with single side polished. I want to have
the other side polished. Do you know any information on companies which
offer this service?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group