MEMSnet Home: MEMS-Talk: re: Any metal as KOH masking layer?
re: Any metal as KOH masking layer?
2005-06-02
Gabriel Matus
re: Any metal as KOH masking layer?
Gabriel Matus
2005-06-02
I've never tried it, but I've heard that Au can serve as an excellent
mask for KOH.  A key point I imagine would be to have a thin, low
stress Cr adhesion layer to minimize undercutting.

Gabriel Matus

>From: "D. Zhou" 
>Subject: [mems-talk] Any metal as KOH masking layer?
>
>I am just wondering if any metal can act as the masking layer( strong
>enough in KOH and easy to be removed) for deep KOH etching (say,~600 um
>deep) at 80 degrees. (It may take about 10 hours to finish the etching
>process). I tried NiCr (50 nm) but it could not sustain after 2 hours.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing