MEMSnet Home: MEMS-Talk: antireflection coating?
PDMS bonding to glass
2005-06-01
[email protected]
2005-06-01
Lee Pang
2005-06-02
[email protected]
antireflection coating?
2005-06-03
[email protected]
2005-06-03
Robert Black
2005-06-07
John Maloney
antireflection coating?
[email protected]
2005-06-03
Hello,

I am working on the two beam interference grating structure with 0.5~1um thick
photoresist. So far I did not use antireflection coating but I cannot still get
grating.
I am just wondering if anyone have any experience about how much differences
between with antireflection coating and without it?
Thanks,


Jason
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing