Au/Cr(or Ti) as the KOH mask
2005-06-08
D. Zhou
2005-06-09
Jessica Gomez
Au/Cr(or Ti) as the KOH mask
D. Zhou
2005-06-08
Dear members,

I deposited a 250nm-thick Si3N4 layer as the mask of KOH but it could not
provide sufficient protection during the KOH ething. This is partly because
SiN deposited in our group is not pure Si3N4, but contains a large amout of
oxygen. The patterns are not well difined using this SiN as the mask.

Now I am going to try some metals as the masking layer, say Au/Cr or Au/Ti
(Cr or Ti works as the adhesive layer). Is there anybody who has any
experiences in this? How thick should the Au layer be so that it can be
strong enough during a very long etch time (9~10 hours in KOH @80c.) Any
suggestions? Thanks a lot.

Daxiang Zhou
Semiconductor Physics Group
Cavendish Laboratory
University of Cambridge
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation