Pyrex/Quarz etching small features
2005-06-08
Daniel Schwaab
2005-06-08
mallikarjun kamavaram
2005-06-08
Robert Black
2005-06-09
mallikarjun kamavaram
Pyrex/Quarz etching small features
Robert Black
2005-06-08
Do you have any more info on your micro sandblasting? What type of equipment
do you use? What do you use as your blasting media?

Robert

-----Original Message-----
From: mallikarjun kamavaram
Subject: Re: [mems-talk] Pyrex/Quarz etching small features

HI DANIEL
I HAVE BEEN WORKING ON NEW MICRO/NANO GRIT SAND BLASTING IT CAN BE
HELPFUL TO GET YOUR REQUIRED DIMENSIONS. IT IS THE EASIEST , FASTEST,
CHEAPEST ONE BUT U SHOULD HAVE THAT EQUIPMENT. AM TELLING YOU COX I
HAVE BEEN WORKING ON THIS.THE ETCH RATE WITH THIS PROCESS IS
800-1000micron/min
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review