Mechanically machining thick [~4 mm] Silicon.
2005-06-15
Alderete, Michael
2005-06-16
Martin Heller
2005-06-16
Shivalik Bakshi
2005-06-16
Paul Hines
2005-06-16
Shay Kaplan
Mechanically machining thick [~4 mm] Silicon.
Paul Hines
2005-06-16
I have machined large fixtures and silicon parts up to 12mm thick using dicing
saws.  These parts
often needed trenches or beveled edges which were not a problem to do.  Contact
me if you need any
help or look up MicroXact.

Good luck!

--
Paul Hines

> Does anyone have experience with the mechanical machining of thick
> [approximately 4 mm thick] Silicon?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing