MEMSnet Home: MEMS-Talk: To achive vertical sidewall of PR after dry etching of oxide
To achive vertical sidewall of PR after dry etching of oxide
2005-06-17
xiaodong wang
To achive vertical sidewall of PR after dry etching ofoxide
2005-06-18
Lou Chomas
PZT dry/wet etch selective to Pt
2005-06-20
Tolga Kaya
To achive vertical sidewall of PR after dry etching of oxide
xiaodong wang
2005-06-17
Hi,

I need help from you guys.

I am dealing with the structure with PR (8 um) on top,
Si dioxide (0.4 um), then silicon substrate.

After developing, I did dry etching of oxide.
The problem  is; after etching, the sidewall (PR) is
not vertical.

Can you have a idea to keep sidewall vertical after
oxide etching?

Any information will be appreciated.

Xiaodong
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Mentor Graphics Corporation