Micro fluidic visualization
Zhiyong Xiao
2005-07-03
Dear all,

I want to visualize DI water or aqueous methanol solution flow in
micro channels formed by silicon-glass bonding. The channel cross
section is around 100umX100um.

Can anyone recommend me a dye that can visualize the micro fluids but
can be easily cleaned away without contaminating the channels after
usage.

I prefer white light source, but fluorescent dye is also a choice if I
have to. Thank you very much!

Best Regards,
Orlando
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics