Conglomeration of Silver-coated Hollow Glass Spheres in µPIV
2005-07-14
Sebastian Große
Conglomeration of Silver-coated Hollow Glass Spheres in µPIV
Sebastian Große
2005-07-14
Hello,
We are using silver-coated hollow glass-spheres with 4µm mean-diameter in
our µPIV-measurements. Unfortunately these particles start conglomerating in
paraffin oil (and water) and they get stuck in our microstructures instead
of just floating around the structures. Has anyone experience in using
silver-coated hollow glass-spheres and knows how to avoid the clustering of
the particles in paraffin/water.
Many thx
Sebastian Große
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.