Problem with Lift-off
2005-07-08
ahajjiah
2005-07-10
Cristi Lepadatu
2005-07-11
William Lanford-Crick
Stability of silane-based SAMs
2005-07-19
Simon Garcia
Stability of silane-based SAMs
Simon Garcia
2005-07-19
Hello,

I would like to functionalize a SiO2/Si or glass surface to improve
film deposition of metal oxides on the substrate. I think SAMs based on
organosilicon molecules, is the best way to go. The problem is that my
film deposition occurs in H2O, at pH=10 and temperature of 75 deg C,
and I'm afraid the basic conditions will attack the monolayer.

Does anyone have experience with organosilane monlayers, and had
problems with stability in aqueous solution?

Where can I find studies on the stability of these monolayers in
different environments?

Thanks,
Simon Garcia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.