MEMSnet Home: MEMS-Talk: Re: RE: SiNx dry etch (William Lanford-Crick)
Re: RE: SiNx dry etch (William Lanford-Crick)
2005-07-24
Michael Marrs
Re: RE: SiNx dry etch (William Lanford-Crick)
Michael Marrs
2005-07-24
Bill-

Methane does not etch silicon nitride at all. In fact, methane is used to
etch certain materials when a high selectivity to silicon nitride is
required. If you want to add a chlorine-containing gas, try adding boron
trichloride. It should etch silicon nitride faster than chlorine.

Regards,

Mike
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Nano-Master, Inc.
Harrick Plasma, Inc.