A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Pyrex wafer anodically bonded to Thin Silicon Problem
Pyrex wafer anodically bonded to Thin Silicon Problem
2005-08-01
Zoberbier, Margarete
2005-08-01
Tony Rogers
Coating of Poly Si with a Ferromag Matl !!!!
2005-08-01
Namit Singh
How to etch Silicon into oblique walls using ICP?
2005-08-01
ning
2005-08-01
Hongjun-ECE
2005-08-02
ning
2005-08-03
David Nemeth
Pyrex wafer anodically bonded to Thin Silicon Problem
Tony Rogers
2005-08-01
Hello Badin,

Restricting the switch-on voltage is even easier with AML bonders which
allow operation in current-limited mode. By operating in this mode you can
ensure that the voltage automatically increases at a rate that matches the
resistivity changes in the glass.

Tony Rogers
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing