I am looking for some advice on removing thin metal layers used as an
underbump metal layer in solder bump deposition.  My underbump metal
composition is:
400A Ti
500A Cu
400A Au
My bumps are PbSn solder.  Obviously, I want to minimize undercutting
the bumps, as well as minimize attack to the solder itself.

Hope someone can help!  Regards,

Keith McConnell
Children's Hospital Med Ctr
Cincinnati,  OH


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing