MEMSnet Home: MEMS-Talk: ICP-RIE coil frequency
any one can suggest some reference or books about ICP etch?
2005-08-25
baobao
ICP-RIE coil frequency
2005-09-08
William Lanford-Crick
2005-09-09
Barry Isenor
ICP-RIE coil frequency
Barry Isenor
2005-09-09
I believe the 13.56 MHz is use to produce high density plasma and the 2 MHz
is used bias the wafer.

-----Original Message-----
From: William Lanford-Crick [mailto:[email protected]]
Sent: September 8, 2005 4:16 PM
To: 'General MEMS discussion'
Subject: [mems-talk] ICP-RIE coil frequency

         Hi Group,

         We have 2 ICP-RIE system.  1 is a PlasmaTherm (now Unaxis), with
the ICP coil at 2 MHz.  The other is an STS Bosch process system with the
coil at 13.56 MHz.  Both system have platen power at 13.56 MHz.

         Can somebody tell me what difference the ICP coil frequency makes?
Why would we want 2 MHz vs. 13.56 Mhz?  Is there an advantage to having the
coil and RIE power at 2 different frequencies?
         Thanks for any info you an supply,

         Bill

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing