A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Rép. : [mems-talk] Oxidize Silicon
Rép. : [mems-talk] Oxidize Silicon
2005-09-09
Laetitia Philippe
Re:Rép.: [mems-talk] Oxidize Silicon
2005-09-09
[email protected]
Re: Rép. : [mems-talk] Oxidize Silicon
2005-09-09
Jim Beall
Re: Rép. : [mems-talk] Oxidize Silicon
2005-09-09
mizur
Re: Rép. : [mems-talk] Oxidize Silicon
Jim Beall
2005-09-09
There is a handy oxidation calculator on-line at:
http://www.lelandstanfordjunior.com/dealgrove.html

On Sep 9, 2005, at 10:13 AM, [email protected] wrote:

> I have Gold pattern on the sample and meling point of Gold is 1064oC.
> if I want to do it at 1000oC or 900oC, what should be the time by your
> expection?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation