2005-09-16
I'm looking for alternative to arch chemical Photoresists.

we use HNR and HPR resists

our volume is low enough that currently we are wasting up to 80% of the because
shelf life is up.
Arch/fuijfilm sells their products in 4 liter batches, and make it 4 times a
year.

The performance of the product is good so I want a product that performs
similarly

our feature size is min~7um and we need excellent resolution. and liter or 500ml
volumes

Cyrus Grimes
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
MEMStaff Inc.