laminate microfluidics
Brubaker Chad
2005-09-28
In terms of a "press" to push the devices together, your best bet is to
use an existing industry resource - wafer bonders such as the EVG520.

Best Regards,
Chad Brubaker


-----Original Message-----
From: Dwayne Dunaway
Sent: Tuesday, September 27, 2005 4:14 PM
To: General MEMS discussion
Subject: [mems-talk] laminate microfluidics


I am interested in making laminate microfluidic devices.

Does anyone have any suggestions for low autofluorescent glue layers?

Also, we need a press to put the devices together.  Any suggestions for
presses?

Are there general references that would describe how to get started with
the process?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.