silicon nitride stress problems
Duan
2005-10-11
Yes, I deposited one side of my wafer(not prime one) with 1um nitride, and
then put it in the oxidation furnace to grow 0.4um oxide on the other side
of my wafer.

On 10/8/05, [email protected]  wrote:
>
> If one side of the wafer has 1um PECVD nitride, nitride will prevent
> oxidation.
> Duan, do you mean get 0.4um oxide from the backside
> of the wafer?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Nano-Master, Inc.