SU8 adhesion
2005-10-12
Lung-hao Hu
2005-10-17
Thomas Xu
2005-10-18
Joseph Grogan
2005-10-18
GARCIA BLANCO Sonia
SU8 adhesion
Lung-hao Hu
2005-10-12
I am using SU-8 to be a mold on glass substrate
and then pour PDMS on the top of this mold to build up a microfludic device.
After developing SU-8, the whole mold is stripped.
The reason why I guess is that the interfacial area bewteen SU-8 and glass is
pretty small, therefore the adhesion is not good.
Is there any product that can enhance the adhesion between SU-8 and glass.

Lunghao

--
Dept.of Mechanical Engineering
Univ. of Colorado Boulder
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation