MEMSnet Home: MEMS-Talk: how to solve wafer conducting problem
how to solve wafer conducting problem
2005-10-13
Jiang Ziling
how to solve wafer conducting problem
Jiang Ziling
2005-10-13
We recently grew some 100um wide, 150nm high, mm-scale long metal contacts
on P-doped Si wafer but found that they are conducting with each other
through the Si wafer at resistances around several hundred ohms. We didn't
find this phenomenon when we directly apply multimeter tip onto the Si wafer
surface to test. I guess this is because the 'large' area of metal contacts
eased conduction through the wafer area between the contacts.
 Does anybody have good idea that what kind of wafer we should use in order
to largely avoid this problem? We don't care whether it is Si or pyrex or
anything else, only if it is flat enough and insulating. And any good
provider of such wafers?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
Addison Engineering