A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to release PDMS from Aluminum mold easily?
How to release PDMS from Aluminum mold easily?
2005-10-12
Jeff chen
2005-10-13
Joseph Grogan
How to release PDMS from Aluminum mold easily?
Joseph Grogan
2005-10-13
Instead of coating, you could try dropping the whole thing in a solvent
such as acetone, which will make the PDMS swell and pop itself off of
the mold. The swelling is reversible so just put the PDMS on a hot plate
to dry off and it will come back to its normal size.

-Joe Grogan

Jeff chen wrote:

>Hi, all,
>
>I am working on the PDMS related project.
>Right now, I met a problem that it is not easy to release the cured
>PDMS from the Aluminum mold.
>Is there any way to do that easily? Like some reagent or a Teflon layer on
>mold?
>Any idea about that?
>
>Thanks a lot.
>
>Best,
>Jifeng
>_______________________________________________
>Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>provider of MEMS and Nanotechnology design and fabrication services.
>Visit us at http://www.mems-exchange.org
>
>Want to advertise to this community?  See http://www.memsnet.org
>
>To unsubscribe:
>http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation