A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Residue with RIE
Residue with RIE
2005-10-13
Jauniskis, Linas
2005-10-13
[email protected]
2005-10-17
Robert Dean
Residue with RIE
Robert Dean
2005-10-17
Linas,

Hi.  You might want to try cleaning out the etching chamber.  O2 based
RIE etching of LCP will, over time, build up residue in the etching
chamber itself which can impede etching.

Sincerely,

Robert Dean
Auburn University

>>> [email protected] 10/13/2005 12:50:43 PM >>>
I am working with a RIE machine O2 etching a thick layer (50um) of an
organic (LCP). After etching through most of the depth, there is a
black
residue left on the sample. My guess is this is oxidation byproducts
from the etch - anyone know with more certainty?

If that's it, what would help sweep the residue out? Increased flow
rate? On this system it appears that all I can do there is hook up a
higher capacity pump in order to increase gas flow rate while keeping
the pressure in the same range.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group