Hi all,
I'm working with PDMS to build thin cantilever beams. Does anyone know how to
lower the viscosity of the PDMS say, Sylgard 184??? I'm using the standard 10:1
ratio one. I'm looking for a thickness less than 1 micron. Please help.

Vinny