MEMSnet Home: MEMS-Talk: Polycarbonate bonding
Polycarbonate bonding
2005-10-28
Peter Svasek
2005-10-28
Jeff chen
Polycarbonate bonding
Jeff chen
2005-10-28
Hi, Peter,

It's pretty easy. Under certain pressure and 150 degree C 20 minutes,
you'll get well binding. Check the reference paper here: Anal.Chem.
2005, 77, 658-666

Good luck.

Best,
Jifeng

On 10/28/05, Peter Svasek  wrote:
> Hi,
>
> is anyone out there who could give me some hints about
> direct bonding of polycarbonate (Lexan) sheets (PC to PC)
> to form microfluidik structures?
> plasma treatment, bond parameters etc ::
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group