Help wanted - plating base layer info!!
2005-11-01
mathew varghese
2005-11-10
Abhinav Bhushan
Help wanted - plating base layer info!!
mathew varghese
2005-11-01
Hello evryone..
  I'm attempting to fabricate a MEMS solenoid inductor with a Cr/Cu/Ni plating
base.Is this step correct or should I use  a Ti/Cu/Cr combination.Could some one
please help me out in this matter and if possible also tell me whether DC
sputtering or electroplating would be a good choice to deposit these films?

Thanking you in anticipation.
Mathew
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.