Thinning SU-8 2002
2005-10-31
[email protected]
2005-11-01
Robert Black
Thinning SU-8 2002
Robert Black
2005-11-01
I don't think you can get SU-8 that thin. I think you'd have to dilute it so
much you'd lose the photo properties. (We use a barc to get a 800nm thick
and it seems about as viscous as water).

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of [email protected]
Sent: Monday, October 31, 2005 4:34 PM
To: [email protected]
Subject: [mems-talk] Thinning SU-8 2002

Hello,

I was wandering if anyone has any experience in thinning SU-8 2000.  I have
SU-8 2002 and the SU-8 2000 thinner.  I would like to be able to spin-on a
100 nm or thinner layer of SU-8, but I don't know if this is even possible.
If anyone has any advice on this or knows how thin I could possibly make a
layer of SU-8, it would be greatly appreciated.  Thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.
Tanner EDA by Mentor Graphics