MEMSnet Home: MEMS-Talk: Deposit passivation layer over SU8
Deposit passivation layer over SU8
2005-11-04
[email protected]
Deposit passivation layer over SU8
[email protected]
2005-11-04
I just wondering if anyone has experiences to deposit a passivation layer
(oxide, nitride) over SU8. How is the adhesion and any stress issues?
Thanks!

Gene