MEMSnet Home: MEMS-Talk: Lift off for oxide mask?
Lift off for oxide mask?
2005-11-07
Pete Kirby
2005-11-08
William Lanford-Crick
Lift off for oxide mask?
William Lanford-Crick
2005-11-08
         You CAN lift-off an oxide mask if the oxide is deposited by
electron-beam lithography.  I don't know if thermal evaporation is
possible--I have not tried it.  However, the quality will not be nearly as
good as a grown oxide.  Grown oxide, such as PECVD, cannot be lifted off
because it would grow conformably around the resist.  In addition, the
growth temperature may well destroy the resist.
         -Bill


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMStaff Inc.