A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SEM Thickness Measurement
SEM Thickness Measurement
2005-11-07
Eric J. Correa
2005-11-08
Trevor Semple
2005-11-08
Hongjun-ECE
2005-11-09
Isaac Wing Tak Chan
SEM Thickness Measurement
Isaac Wing Tak Chan
2005-11-09
Eric,

If it is a wafer, for better result of course you use a dicing saw to cut
the back side of your wafer but leave some height uncut to create a
scribe line. Then use a roller to press again the front side of the wafer
to cleave your wafer. Cutting the film directly will not give clean cross
section. Or, you make two molds that you can just insert the wafer on both
ends (like paper inserts into an envelope), then you can use both hands to
snap the wafer.

Yours sincerely,

Isaac Chan, PhD
University of Waterloo
"Innovate. Lead. Succeed."

On Mon, 7 Nov 2005, Eric J. Correa wrote:

> Hi Everyone:
>
> I am trying to measure UNCD (diamond) thickness using a SEM
> by looking at the cross sectional area.  I am using a
> diamond tip to cut my samples but I am not able to get a
> clean cross-sectional area.  I was just wondering if anyone
> has any advice or recommendation.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation