MEMSnet Home: MEMS-Talk: one more wax question
one more wax question
2005-11-10
Abhinav Bhushan
2005-11-10
Brent Garber
2005-11-10
Ad Hall
2005-11-11
David Henriks
Process control
2005-11-11
jedidi nader
2005-11-12
PRAMOD GUPTA
Wet Etchant for silicon nitride
2005-11-20
Roger Brennan
2005-11-21
Carel Heerkens
EPON SU8
2005-11-21
Ladan Abolghasemi
2005-11-10
Adamson, Steve
one more wax question
David Henriks
2005-11-11
We offer several different types of wax with different melting points and
requiring different solvents.  All waxes clean off very well.  Of particular
interest will be our MWH135 mounting wax which has a melting point of about 135
C and is soluble in acetone.  Our MWM100 is a Black Wax that melts at about 100C
and is resistant to most etching solutions.  It can be removed with hydrocarbon
or chlorinated solvents.  If you have an interest, I would be pleased to discuss
this off-line and send you samples of the various waxes we have.

Abhinav Bhushan wrote:

>Hi,
>
>I want to use wax as a sacrificial material. I am
>looking for one
>which will melt at >100 C, preferably 125 C, and which
>can be
>dissolved in a solvent (acetone, hexane, etc). I was
>wondering if
>anyone has worked with or looked into a product like
>this. I looked
>online for wax, most of the ones available were used
>for mounting
>samples, I am not sure how clean the surface would be
>after removing
>the wax. The wax I have right now melts at 60 C, so I
>cant use it the
>way I want to. I will appreciate any help.
>

--
David Henriks

South Bay Technology, Inc.
1120 Via Callejon
San Clemente, CA 92673 USA

TEL: +1-949-492-2600
Toll-free in the USA: +1-800-728-2233
FAX: +1-949-492-1499

email: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation