Hi Pawel,

If you are interested in teflon-like coating (hydrophobic, low surface
energy) you can use self-assembled monolayers (SAMs), which can be deposited
from a vapor phase by commercially available systems, like MVD-100. These
systems are installed at the following facilities (MEMS-exchange network):
UC Berkeley, Cornell University, etc. If you have troubles to get there you
may also contact me directly and I will arrange coating run for you.

Regards,
Boris Kobrin
Applied Microstructures, Inc.
[email protected]
(408) 594-0654

------------------------------

Message: 5
Date: Fri, 18 Nov 2005 08:00:39 +0100
From: Pawel Janus 
Subject: [mems-talk] PTFE coating
To: [email protected]
Message-ID: <[email protected]>
Content-Type: text/plain; charset=ISO-8859-1; format=flowed

Hi all,
I'm looking for PTFE coating provider. I'd like to deposit teflon on
silicon/silicon dioxide layer. I would be grateful for any information.

Regards
Pawel

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.