MEMSnet Home: MEMS-Talk: PDMS binding to GLASS
PDMS binding to GLASS
2005-11-19
suppi
2005-11-19
[email protected]
2005-11-20
karim faid
2005-11-21
Lee Pang
2005-11-21
Beggans Michael H IHMD
PDMS binding to GLASS
karim faid
2005-11-20
Hi:
  One way around using the plasma, is to use an uncured PDMS solution sandwiched
between your PDMS material and the glass and cure it while applying a gentle
pressure. You can improve the bonding by cleaning the glass in a piranha
solution (to render it hydrophilic) and by using a PDMS material that is only
partially cured.
  Karim

[email protected] wrote:
  I have heard this is acid method to do this, but I've never found it.

> Hi all,
>
> I want to irreversibly bind PDMS to Glass but do not have a plasma
> cleaner.
> IS there any other method of doing it.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing