A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Crosslink PMMA
SiO2 hydrophilic enhanced?
2005-11-07
Wullinger, Michaela
2005-11-07
Shay Kaplan
HD-8820 Polyimide
2005-11-07
Giuliano Gregori
2005-11-08
walter
2005-11-07
ssood
2005-11-07
sokwon Paik
Crosslink PMMA
2005-12-01
[email protected]
2005-12-02
Fabio Altomare
anodic bonding question
2005-12-02
Robert Dean
2005-12-03
Kirt Williams
anodic bonding: contaminants at glass top surface
2005-12-20
Antonius Helvoort
2005-12-21
Shay Kaplan
2005-12-21
Shile
2005-11-07
Gary
Crosslink PMMA
[email protected]
2005-12-01
Hello all:

I want to crosslink PMMA and I know high dose e-beam exposure can do
this.
but what I want is to cross link large area of PMMA which can not be
done by e-beam.

can UV work? somebody asked this before but I could not find the
answer.

what should be the condition?

any suggestions are welcome.

best

Yu Chen
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering