MEMSnet Home: MEMS-Talk: evenly distribute micrometer size Red Iron Oxide partibles
evenly distribute micrometer size Red Iron Oxide partibles
2005-12-03
张 勐
evenly distribute micrometer size Red Iron Oxide partibles
张 勐
2005-12-03
Hi all,

I want to distribute the Red iron oxide partibles very evenly on a PDMS
surface. Can anybody here give me some help? Thanks a lot.