MEMSnet Home: MEMS-Talk: Alignment on E-beam Writing
Alignment on E-beam Writing
2006-01-18
Z Destro
2006-01-18
[email protected]
2006-01-18
Hongjun-ECE
Alignment on E-beam Writing
[email protected]
2006-01-18
you can write an alignment mark and evaporated metal like Au which is
easy to see for the next writing.

best

Yu Chen



Quoting Z Destro :

> Hi all,
> I am wondering how to make the alignment when we are trying to make
> multilayers using e-beam lithography. as for photolithography, we can use
> alignment mark on masks to make sure the structure on different layers are
> correctly aligned. but for E-beam lighography, I have no idea. Could anyone
> explain it for me?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation