MEMSnet Home: MEMS-Talk: Selective, clean PDMS etch
Selective, clean PDMS etch
2006-01-20
[email protected]
Selective, clean PDMS etch
[email protected]
2006-01-20
Hi, Rick,
I saw your post on mems-talk. have you been able to find a good receipe for
RIE over PDMS? If so, do you mind sharing your success stories? Thanks. I am
trying to etch pdms too, but need some help.
--
Best Regards,
Yu Xiang
reply