Pin holes' problem in Gold
2006-01-24
Manoj Wadhwa
Pin holes' problem in Gold
Manoj Wadhwa
2006-01-24
I am doing bulk-micromacining of silicon structure in KOH, protecting the
structure with Chrome- Gold(1 micron thick - ebeam evaporated ;using lift off
process). After bulk-micromachining I find bubbles in gold layer(may be because
of pin holes) and silicon is getting attacked. Can someone suggest how to get
rid of these pin holes?

Thanks & Regards!

Manoj Wadhwa
SCL-India
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Addison Engineering
MEMS Technology Review