MEMSnet Home: MEMS-Talk: Gold patterning using lift off on substrates
Gold patterning using lift off on substrates
2006-01-24
Gabe Dagani
2006-01-25
Hongjun-ECE
2006-01-25
Silvan Schmid
2006-01-25
Tao
Does S1818 developer attack PMMA?
2006-01-25
sokwon Paik
2006-01-25
Bill Moffat
Gold patterning using lift off on substrates
Gabe Dagani
2006-01-24
I was interested if anyone had a particular resist they used for a lift off
process of Cr/Au pads on glass slides or on PDMS.

Process that I would like to perform:

1) Clean substrate
2) Dry, perhaps HMDS
3) Spin PR (What PR is good?)
4) Develop
5) Evaporate Cr/Au on substrate
6) Lift off the PR to expose just substrate and Cr/Au

Has anyone tried this or have suggestions?

I don't know what PR is good for glass slides or PDMS

 - thanks - Gabe Dagani

  UT Austin, NNIN MRC

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Mentor Graphics Corporation
University Wafer