MEMSnet Home: MEMS-Talk: contrast in PDMS
contrast in PDMS
2006-01-26
Gabe Dagani
contrast in PDMS
Gabe Dagani
2006-01-26
Greetings,

        Has anyone tried putting particles inside the PDMS mixture to
provide optical contrast? I am looking to make PDMS have a dark background
for imaging by means of either coating channels with film (metal or carbon,
etc), or by mixing in colloids to create a dark suspension.

            Thanks in advance.

            Gabe Dagani

            NNIN UT Austin.